Specialty metal and alloy prices (USD/kg)
Published Daily published values, not live quotesnot live quotes
Inconel MA6000
available to members
Latest publication 20 Nov 2026priced every business day since 2 Jan 2019
SuperMetalPrice publishes one price per business day for 1,185 specialty metals and alloys: 64 materials and 1,121 alloys. Each alloy is priced from the day's material prices and its recipe. The 14 Base Metal and Precious Metal prices are open to everyone; the others are available to members.
Base Metal
7 itemsFree| Name | Price USD/kg | Change | 30 days | Published |
|---|---|---|---|---|
| Al Aluminium | 3.185 | up 2.56 percent | ||
| Cu Copper | 12.23 | down 2.70 percent | ||
| Fe Iron | 0.4765 | down 0.52 percent | ||
| Ni Nickel | 15.31 | down 0.75 percent | ||
| Pb Lead | 1.825 | up 0.16 percent | ||
| Sn Tin | 41.16 | down 2.46 percent | ||
| Zn Zinc | 3.67 | down 1.20 percent |
Precious Metal
7 itemsFree| Name | Price USD/kg | Change | 30 days | Published |
|---|---|---|---|---|
| Ag Silver | 1,351.94 | down 1.38 percent | ||
| Au Gold | 114,344.29 | down 0.83 percent | ||
| Ir Iridium | 326,332.98 | unchanged | ||
| Pd Palladium | 29,289.59 | down 6.47 percent | ||
| Pt Platinum | 42,540.20 | up 0.33 percent | ||
| Rh Rhodium | 289,356.30 | unchanged | ||
| Ru Ruthenium | 59,479.41 | unchanged |
Aluminium Alloy
85 items| Name | Price USD/kg | Change | 30 days | Published |
|---|---|---|---|---|
| 2011 | Members | 20 Nov 2026 | ||
| 2014 | Members | 20 Nov 2026 | ||
| 2017 | Members | 20 Nov 2026 | ||
| 2024 | Members | 20 Nov 2026 | ||
| 208 | Members | 20 Nov 2026 | ||
| 2090 | Members | 20 Nov 2026 | ||
| 2091 | Members | 20 Nov 2026 | ||
| 2099 | Members | 20 Nov 2026 | ||
| 2117 | Members | 20 Nov 2026 | ||
| 2195 | Members | 20 Nov 2026 | ||
| 2219 | Members | 20 Nov 2026 | ||
| 242 | Members | 20 Nov 2026 | ||
| 2618 | Members | 20 Nov 2026 | ||
| 3003 | Members | 20 Nov 2026 | ||
| 3004 | Members | 20 Nov 2026 | ||
| 3105 | Members | 20 Nov 2026 | ||
| 319 | Members | 20 Nov 2026 | ||
| 332 (F332 piston alloy) | Members | 20 Nov 2026 | ||
| 336 (LM13 piston alloy) | Members | 20 Nov 2026 | ||
| 354 | Members | 20 Nov 2026 | ||
| 355 | Members | 20 Nov 2026 | ||
| 359 | Members | 20 Nov 2026 | ||
| 383 | Members | 20 Nov 2026 | ||
| 4032 | Members | 20 Nov 2026 | ||
| 4043 | Members | 20 Nov 2026 | ||
| 4047 | Members | 20 Nov 2026 | ||
| 4145 | Members | 20 Nov 2026 | ||
| 5005 | Members | 20 Nov 2026 | ||
| 5052 | Members | 20 Nov 2026 | ||
| 5059 | Members | 20 Nov 2026 | ||
| 5083 | Members | 20 Nov 2026 | ||
| 5086 | Members | 20 Nov 2026 | ||
| 514 | Members | 20 Nov 2026 | ||
| 5154 | Members | 20 Nov 2026 | ||
| 518 | Members | 20 Nov 2026 | ||
| 5182 | Members | 20 Nov 2026 | ||
| 535 (Almag 35) | Members | 20 Nov 2026 | ||
| 5356 | Members | 20 Nov 2026 | ||
| 5454 | Members | 20 Nov 2026 | ||
| 5456 | Members | 20 Nov 2026 | ||
| 5754 | Members | 20 Nov 2026 | ||
| 6005 | Members | 20 Nov 2026 | ||
| 6013 | Members | 20 Nov 2026 | ||
| 6060 | Members | 20 Nov 2026 | ||
| 6061 | Members | 20 Nov 2026 | ||
| 6063 | Members | 20 Nov 2026 | ||
| 6066 | Members | 20 Nov 2026 | ||
| 6082 | Members | 20 Nov 2026 | ||
| 6262 | Members | 20 Nov 2026 | ||
| 6351 | Members | 20 Nov 2026 | ||
| 7005 | Members | 20 Nov 2026 | ||
| 7010 | Members | 20 Nov 2026 | ||
| 7020 | Members | 20 Nov 2026 | ||
| 7039 | Members | 20 Nov 2026 | ||
| 7049 | Members | 20 Nov 2026 | ||
| 7050 | Members | 20 Nov 2026 | ||
| 7055 | Members | 20 Nov 2026 | ||
| 7068 | Members | 20 Nov 2026 | ||
| 7072 (clad) | Members | 20 Nov 2026 | ||
| 7075 | Members | 20 Nov 2026 | ||
| 7085 | Members | 20 Nov 2026 | ||
| 713 (Tenzaloy) | Members | 20 Nov 2026 | ||
| 7150 | Members | 20 Nov 2026 | ||
| 7178 | Members | 20 Nov 2026 | ||
| 7475 | Members | 20 Nov 2026 | ||
| 8006 | Members | 20 Nov 2026 | ||
| 8011 | Members | 20 Nov 2026 | ||
| 8090 | Members | 20 Nov 2026 | ||
| 850 (Al-Sn bearing alloy) | Members | 20 Nov 2026 | ||
| A201 (Al-Cu-Ag) | Members | 20 Nov 2026 | ||
| A206 | Members | 20 Nov 2026 | ||
| A356 | Members | 20 Nov 2026 | ||
| A357 | Members | 20 Nov 2026 | ||
| A360 | Members | 20 Nov 2026 | ||
| A380 | Members | 20 Nov 2026 | ||
| A413 | Members | 20 Nov 2026 | ||
| ADC12 | Members | 20 Nov 2026 | ||
| Al-10Ce Master Alloy | Members | 20 Nov 2026 | ||
| Al-10La Master Alloy | Members | 20 Nov 2026 | ||
| Al-10Ti Master Alloy | Members | 20 Nov 2026 | ||
| Al-10Y Master Alloy | Members | 20 Nov 2026 | ||
| Al-25Mn Master Alloy | Members | 20 Nov 2026 | ||
| Al-50Cu Master Alloy | Members | 20 Nov 2026 | ||
| AlSi10Mg | Members | 20 Nov 2026 | ||
| B390 | Members | 20 Nov 2026 |
Cobalt Alloy
40 items| Name | Price USD/kg | Change | 30 days | Published |
|---|---|---|---|---|
| Co-Cr-W-Mo Dental Ceramic Alloy | Members | 20 Nov 2026 | ||
| CoNiCrAlY Bond Coat (Co-32Ni-21Cr-8Al-0.5Y) | Members | 20 Nov 2026 | ||
| ECY 768 | Members | 20 Nov 2026 | ||
| Elgiloy / Phynox | Members | 20 Nov 2026 | ||
| F-75 | Members | 20 Nov 2026 | ||
| FSX 414 | Members | 20 Nov 2026 | ||
| FSX 430 | Members | 20 Nov 2026 | ||
| Havar | Members | 20 Nov 2026 | ||
| Haynes NS-163 | Members | 20 Nov 2026 | ||
| HS 188 | Members | 20 Nov 2026 | ||
| HS 21 | Members | 20 Nov 2026 | ||
| HS 25 (L605) | Members | 20 Nov 2026 | ||
| HS 31 (X40) | Members | 20 Nov 2026 | ||
| HS 6 | Members | 20 Nov 2026 | ||
| HS 6B | Members | 20 Nov 2026 | ||
| Mar-M 302 | Members | 20 Nov 2026 | ||
| Mar-M 509 | Members | 20 Nov 2026 | ||
| Mar-M 918 | Members | 20 Nov 2026 | ||
| MP159 | Members | 20 Nov 2026 | ||
| MP35N | Members | 20 Nov 2026 | ||
| S-816 | Members | 20 Nov 2026 | ||
| Stellite 1 | Members | 20 Nov 2026 | ||
| Stellite 12 | Members | 20 Nov 2026 | ||
| Stellite 19 | Members | 20 Nov 2026 | ||
| Stellite 190 | Members | 20 Nov 2026 | ||
| Stellite 20 | Members | 20 Nov 2026 | ||
| Stellite 306 | Members | 20 Nov 2026 | ||
| Stellite 4 | Members | 20 Nov 2026 | ||
| Stellite 694 | Members | 20 Nov 2026 | ||
| Stellite 712 | Members | 20 Nov 2026 | ||
| Stellite F | Members | 20 Nov 2026 | ||
| Tribaloy T-400 | Members | 20 Nov 2026 | ||
| Tribaloy T-400C | Members | 20 Nov 2026 | ||
| Tribaloy T-401 | Members | 20 Nov 2026 | ||
| Tribaloy T-800 | Members | 20 Nov 2026 | ||
| Tribaloy T-900 | Members | 20 Nov 2026 | ||
| Ultimet | Members | 20 Nov 2026 | ||
| Umco-50 | Members | 20 Nov 2026 | ||
| WI-52 | Members | 20 Nov 2026 | ||
| X-45 | Members | 20 Nov 2026 |
Copper Alloy
104 itemsFerro Alloy
10 items| Name | Price USD/kg | Change | 30 days | Published |
|---|---|---|---|---|
| Fe-B | Members | 20 Nov 2026 | ||
| Fe-Cr (HC) | Members | 20 Nov 2026 | ||
| Fe-Cr (LC) | Members | 20 Nov 2026 | ||
| Fe-Mn | Members | 20 Nov 2026 | ||
| Fe-Mo | Members | 20 Nov 2026 | ||
| Fe-Nb | Members | 20 Nov 2026 | ||
| Fe-Si | Members | 20 Nov 2026 | ||
| Fe-Ti | Members | 20 Nov 2026 | ||
| Fe-W | Members | 20 Nov 2026 | ||
| FeV | Members | 20 Nov 2026 |
Functional Alloy
36 itemsGold Alloy
36 items| Name | Price USD/kg | Change | 30 days | Published |
|---|---|---|---|---|
| 10K White Gold (Ni) | Members | 20 Nov 2026 | ||
| 10K Yellow Gold | Members | 20 Nov 2026 | ||
| 12K Red Gold (Au-Cu 50/50) | Members | 20 Nov 2026 | ||
| 14K Rose Gold | Members | 20 Nov 2026 | ||
| 14K White Gold (Ni) | Members | 20 Nov 2026 | ||
| 14K White Gold (Pd) | Members | 20 Nov 2026 | ||
| 14K Yellow Gold | Members | 20 Nov 2026 | ||
| 18K Green Gold (Au-Ag 75/25) | Members | 20 Nov 2026 | ||
| 18K Pale Yellow Gold (2N) | Members | 20 Nov 2026 | ||
| 18K Pink Gold (4N) | Members | 20 Nov 2026 | ||
| 18K Rose Gold (5N) | Members | 20 Nov 2026 | ||
| 18K White Gold (Au-Pd) | Members | 20 Nov 2026 | ||
| 18K White Gold (Ni) | Members | 20 Nov 2026 | ||
| 18K Yellow Gold (3N) | Members | 20 Nov 2026 | ||
| 21K Yellow Gold | Members | 20 Nov 2026 | ||
| 22K Yellow Gold | Members | 20 Nov 2026 | ||
| 9K Yellow Gold | Members | 20 Nov 2026 | ||
| Au-Ge 88/12 | Members | 20 Nov 2026 | ||
| Au-Pd Ceramic Alloy (Dental) | Members | 20 Nov 2026 | ||
| Au-Pt 70/30 Dental | Members | 20 Nov 2026 | ||
| Au-Si 97/3 | Members | 20 Nov 2026 | ||
| Au-Sn 80/20 | Members | 20 Nov 2026 | ||
| BAu-1 (37.5Au-62.5Cu) | Members | 20 Nov 2026 | ||
| BAu-2 (80Au-20Cu) | Members | 20 Nov 2026 | ||
| BAu-3 (35Au-62Cu-3Ni) | Members | 20 Nov 2026 | ||
| BAu-4 (82Au-18Ni) | Members | 20 Nov 2026 | ||
| BAu-5 (30Au-36Ni-34Pd) | Members | 20 Nov 2026 | ||
| BAu-6 (70Au-22Ni-8Pd) | Members | 20 Nov 2026 | ||
| BAu-8 (92Au-8Pd) | Members | 20 Nov 2026 | ||
| BVAu-7 (50Au-25Ni-25Pd) | Members | 20 Nov 2026 | ||
| BVAu-9 (35Au-65Cu) | Members | 20 Nov 2026 | ||
| Dental Gold Type I | Members | 20 Nov 2026 | ||
| Dental Gold Type II | Members | 20 Nov 2026 | ||
| Dental Gold Type III | Members | 20 Nov 2026 | ||
| Dental Gold Type IV | Members | 20 Nov 2026 | ||
| Electrum (Au-Ag 80/20) | Members | 20 Nov 2026 |
Low-Melting Alloy
68 items| Name | Price USD/kg | Change | 30 days | Published |
|---|---|---|---|---|
| ACuZinc 5 (Zn-5Cu-3Al) | Members | 20 Nov 2026 | ||
| Bi-Ag 89/11 | Members | 20 Nov 2026 | ||
| Bi-Ag 97.5/2.5 | Members | 20 Nov 2026 | ||
| Bi-In-Sn 57/26/17 | Members | 20 Nov 2026 | ||
| Bi-Pb 55.5/44.5 | Members | 20 Nov 2026 | ||
| Bi-Pb-Sn 52/32/16 | Members | 20 Nov 2026 | ||
| Cd-Ag 95/5 | Members | 20 Nov 2026 | ||
| Cd-Zn 82.5/17.5 | Members | 20 Nov 2026 | ||
| Cerrolow 117 | Members | 20 Nov 2026 | ||
| Cerrolow 136 | Members | 20 Nov 2026 | ||
| Cerrosafe (42.5Bi-37.7Pb-11.3Sn-8.5Cd) | Members | 20 Nov 2026 | ||
| Field's Metal | Members | 20 Nov 2026 | ||
| Ga-In 75.5/24.5 (EGaIn) | Members | 20 Nov 2026 | ||
| Galfan (Zn-5Al) | Members | 20 Nov 2026 | ||
| Galinstan | Members | 20 Nov 2026 | ||
| Galvalume (55Al-Zn-Si) | Members | 20 Nov 2026 | ||
| In-Ag 90/10 | Members | 20 Nov 2026 | ||
| In-Ag 97/3 | Members | 20 Nov 2026 | ||
| In-Bi 66.3/33.7 | Members | 20 Nov 2026 | ||
| In-Pb 50/50 | Members | 20 Nov 2026 | ||
| In-Pb 60/40 | Members | 20 Nov 2026 | ||
| In-Pb-Ag 80/15/5 | Members | 20 Nov 2026 | ||
| In-Sn 52/48 | Members | 20 Nov 2026 | ||
| Pb-Ag 97.5/2.5 (Ag2.5) | Members | 20 Nov 2026 | ||
| Pb-In 75/25 | Members | 20 Nov 2026 | ||
| Pb-Sn 60/40 (Sn40) | Members | 20 Nov 2026 | ||
| Pb-Sn 70/30 (Sn30) | Members | 20 Nov 2026 | ||
| Pb-Sn 80/20 (Sn20) | Members | 20 Nov 2026 | ||
| Pb-Sn 90/10 (Sn10) | Members | 20 Nov 2026 | ||
| Pb-Sn 95/5 (Sn5) | Members | 20 Nov 2026 | ||
| Pb-Sn-Ag 88/10/2 | Members | 20 Nov 2026 | ||
| Pb-Sn-Ag 92.5/5/2.5 | Members | 20 Nov 2026 | ||
| Pb-Sn-Ag 97.5/1/1.5 (Ag1.5) | Members | 20 Nov 2026 | ||
| Rose's Metal | Members | 20 Nov 2026 | ||
| SAC0307 | Members | 20 Nov 2026 | ||
| SAC105 | Members | 20 Nov 2026 | ||
| SAC305 | Members | 20 Nov 2026 | ||
| SAC387 | Members | 20 Nov 2026 | ||
| SAC405 | Members | 20 Nov 2026 | ||
| Sn-Ag 95/5 | Members | 20 Nov 2026 | ||
| Sn-Ag 96.5/3.5 | Members | 20 Nov 2026 | ||
| Sn-Ag-Cu-Bi 93.5/3/0.5/3 | Members | 20 Nov 2026 | ||
| Sn-Bi 42/58 | Members | 20 Nov 2026 | ||
| Sn-Bi-Ag 42/57/1 | Members | 20 Nov 2026 | ||
| Sn-Cu 99.3/0.7 | Members | 20 Nov 2026 | ||
| Sn-In 50/50 | Members | 20 Nov 2026 | ||
| Sn-Pb 50/50 (Sn50) | Members | 20 Nov 2026 | ||
| Sn-Pb 60/40 (Sn60) | Members | 20 Nov 2026 | ||
| Sn-Pb 63/37 (Sn63) | Members | 20 Nov 2026 | ||
| Sn-Pb 70/30 (Sn70) | Members | 20 Nov 2026 | ||
| Sn-Pb-Ag 62/36/2 | Members | 20 Nov 2026 | ||
| Sn-Pb-Bi 43/43/14 | Members | 20 Nov 2026 | ||
| Sn-Zn 91/9 | Members | 20 Nov 2026 | ||
| Sn-Zn-Bi 89/8/3 | Members | 20 Nov 2026 | ||
| Wood's Metal (Cerrobend) | Members | 20 Nov 2026 | ||
| ZA-12 | Members | 20 Nov 2026 | ||
| ZA-27 | Members | 20 Nov 2026 | ||
| ZA-8 | Members | 20 Nov 2026 | ||
| Zamak 2 | Members | 20 Nov 2026 | ||
| Zamak 3 | Members | 20 Nov 2026 | ||
| Zamak 5 | Members | 20 Nov 2026 | ||
| Zinc Anode (ASTM B418 Type I) | Members | 20 Nov 2026 | ||
| Zn-11Al-3Mg-Si Coating (Super Dyma type) | Members | 20 Nov 2026 | ||
| Zn-15Al (Thermal Spray) | Members | 20 Nov 2026 | ||
| Zn-22Al (Superplastic) | Members | 20 Nov 2026 | ||
| Zn-Al-Mg Coating (ZAM 6/3) | Members | 20 Nov 2026 | ||
| Zn-Al-Mg Coating (ZM 1.5/1.5) | Members | 20 Nov 2026 | ||
| Zn-Cu-Ti (Titanium Zinc) | Members | 20 Nov 2026 |
Magnesium Alloy
28 items| Name | Price USD/kg | Change | 30 days | Published |
|---|---|---|---|---|
| AE42 | Members | 20 Nov 2026 | ||
| AE44 | Members | 20 Nov 2026 | ||
| AM100A | Members | 20 Nov 2026 | ||
| AM20 | Members | 20 Nov 2026 | ||
| AM50A | Members | 20 Nov 2026 | ||
| AM60B | Members | 20 Nov 2026 | ||
| AS21 | Members | 20 Nov 2026 | ||
| AS41B | Members | 20 Nov 2026 | ||
| AZ31B | Members | 20 Nov 2026 | ||
| AZ61A | Members | 20 Nov 2026 | ||
| AZ63A | Members | 20 Nov 2026 | ||
| AZ80A | Members | 20 Nov 2026 | ||
| AZ91D | Members | 20 Nov 2026 | ||
| AZ92A | Members | 20 Nov 2026 | ||
| Elektron 21 | Members | 20 Nov 2026 | ||
| EZ33A | Members | 20 Nov 2026 | ||
| LA141A | Members | 20 Nov 2026 | ||
| LZ91 (Mg-9Li-1Zn) | Members | 20 Nov 2026 | ||
| M1A | Members | 20 Nov 2026 | ||
| QE22A | Members | 20 Nov 2026 | ||
| WE43 | Members | 20 Nov 2026 | ||
| WE54 | Members | 20 Nov 2026 | ||
| ZC63A | Members | 20 Nov 2026 | ||
| ZE41A | Members | 20 Nov 2026 | ||
| ZE63A | Members | 20 Nov 2026 | ||
| ZK60A | Members | 20 Nov 2026 | ||
| ZK61A | Members | 20 Nov 2026 | ||
| ZM21 | Members | 20 Nov 2026 |
Magnetic & Electrical Alloy
66 items| Name | Price USD/kg | Change | 30 days | Published |
|---|---|---|---|---|
| Alloy 42-6 (Ni-Fe-Cr sealing) | Members | 20 Nov 2026 | ||
| Alloy 46 (46Ni-Fe) | Members | 20 Nov 2026 | ||
| Alloy 48 (48Ni-Fe) | Members | 20 Nov 2026 | ||
| Alloy 52 (50.5Ni-Fe) | Members | 20 Nov 2026 | ||
| Alnico 1 | Members | 20 Nov 2026 | ||
| Alnico 2 | Members | 20 Nov 2026 | ||
| Alnico 3 | Members | 20 Nov 2026 | ||
| Alnico 4 | Members | 20 Nov 2026 | ||
| Alnico 5 | Members | 20 Nov 2026 | ||
| Alnico 6 | Members | 20 Nov 2026 | ||
| Alnico 8 | Members | 20 Nov 2026 | ||
| Alnico 8HC | Members | 20 Nov 2026 | ||
| Alumel (Type K -) | Members | 20 Nov 2026 | ||
| Chromel (Type K +) | Members | 20 Nov 2026 | ||
| Constantan | Members | 20 Nov 2026 | ||
| CuNi23 Resistance Alloy | Members | 20 Nov 2026 | ||
| CuNi6 Resistance Alloy | Members | 20 Nov 2026 | ||
| Cunife | Members | 20 Nov 2026 | ||
| Electrical Steel (3 % Si) | Members | 20 Nov 2026 | ||
| Electrical Steel (6.5 % Si) | Members | 20 Nov 2026 | ||
| Evanohm | Members | 20 Nov 2026 | ||
| Fe-17Co (Vacoflux 17 type) | Members | 20 Nov 2026 | ||
| Fe-Cr-Co 28/15 | Members | 20 Nov 2026 | ||
| Fe-Cr-Co 28/8 (Arnokrome 3) | Members | 20 Nov 2026 | ||
| Fe-Cr-Co 30/25 | Members | 20 Nov 2026 | ||
| FeCrAl 13-4 (Alkrothal type) | Members | 20 Nov 2026 | ||
| FeCrAl 22-5 (Kanthal D type) | Members | 20 Nov 2026 | ||
| FeCrAl 22-6 (Kanthal A-1 type) | Members | 20 Nov 2026 | ||
| FeCrAl APMT | Members | 20 Nov 2026 | ||
| Finemet (Fe-Si-B-Nb-Cu nanocrystalline) | Members | 20 Nov 2026 | ||
| Galfenol (Fe-17Ga) | Members | 20 Nov 2026 | ||
| Hiperco 27 | Members | 20 Nov 2026 | ||
| Hiperco 50 / 50A (Permendur 2V) | Members | 20 Nov 2026 | ||
| Hy-Mu 80 | Members | 20 Nov 2026 | ||
| Invar 36 | Members | 20 Nov 2026 | ||
| Invar 42 | Members | 20 Nov 2026 | ||
| Karma | Members | 20 Nov 2026 | ||
| Kovar | Members | 20 Nov 2026 | ||
| Manganin | Members | 20 Nov 2026 | ||
| Metglas 2605SA1 (Fe-Si-B amorphous) | Members | 20 Nov 2026 | ||
| Metglas 2826MB (Fe-Ni-Mo-B amorphous) | Members | 20 Nov 2026 | ||
| MPP Core Alloy (Ni-17Fe-2Mo) | Members | 20 Nov 2026 | ||
| Mu-metal | Members | 20 Nov 2026 | ||
| Mumetal (Ni-Cu-Cr type) | Members | 20 Nov 2026 | ||
| Nd-Ce-Fe-B (sintered, Ce-substituted) | Members | 20 Nov 2026 | ||
| Nd-Fe-B (bonded, isotropic powder) | Members | 20 Nov 2026 | ||
| Nd-Fe-B (sintered, EH/AH ultra-high coercivity) | Members | 20 Nov 2026 | ||
| Nd-Fe-B (sintered, high coercivity SH/UH) | Members | 20 Nov 2026 | ||
| Nd-Fe-B (sintered, standard) | Members | 20 Nov 2026 | ||
| Nd-Pr-Fe-B (sintered, didymium) | Members | 20 Nov 2026 | ||
| Ni-Span-C 902 | Members | 20 Nov 2026 | ||
| Nichrome (80-20) | Members | 20 Nov 2026 | ||
| Nichrome 35/20 (35Ni-20Cr-Fe) | Members | 20 Nov 2026 | ||
| Nichrome 60/15 | Members | 20 Nov 2026 | ||
| Nichrome 70/30 | Members | 20 Nov 2026 | ||
| Nicrosil (Type N +) | Members | 20 Nov 2026 | ||
| Nifethal 70 (Ni-28Fe) | Members | 20 Nov 2026 | ||
| Nisil (Type N -) | Members | 20 Nov 2026 | ||
| Pt-Co Magnet (77/23) | Members | 20 Nov 2026 | ||
| Sendust (Fe-Si-Al) | Members | 20 Nov 2026 | ||
| Sm-Co 1:5 (SmCo5) | Members | 20 Nov 2026 | ||
| Sm-Co 2:17 (Sm2Co17) | Members | 20 Nov 2026 | ||
| Super Invar 32-5 | Members | 20 Nov 2026 | ||
| Terfenol-D | Members | 20 Nov 2026 | ||
| Vicalloy (Fe-Co-V semi-hard) | Members | 20 Nov 2026 | ||
| Zeranin 30 (Cu-7Mn-2.3Sn) | Members | 20 Nov 2026 |
Nickel Alloy
67 items| Name | Price USD/kg | Change | 30 days | Published |
|---|---|---|---|---|
| 45Ni35CrNb | Members | 20 Nov 2026 | ||
| 50Ni50CrNb | Members | 20 Nov 2026 | ||
| Alloy 20 | Members | 20 Nov 2026 | ||
| Alloy 2120 MoN | Members | 20 Nov 2026 | ||
| Alloy 28 | Members | 20 Nov 2026 | ||
| Alloy 31 | Members | 20 Nov 2026 | ||
| Alloy 33 | Members | 20 Nov 2026 | ||
| Alloy 45TM | Members | 20 Nov 2026 | ||
| Alloy 59 | Members | 20 Nov 2026 | ||
| Alloy 699 XA | Members | 20 Nov 2026 | ||
| CZ-100 (cast nickel) | Members | 20 Nov 2026 | ||
| Duranickel 301 | Members | 20 Nov 2026 | ||
| Hastelloy B (2) | Members | 20 Nov 2026 | ||
| Hastelloy B-3 | Members | 20 Nov 2026 | ||
| Hastelloy C 22 | Members | 20 Nov 2026 | ||
| Hastelloy C 276 | Members | 20 Nov 2026 | ||
| Hastelloy C 4 | Members | 20 Nov 2026 | ||
| Hastelloy C-2000 | Members | 20 Nov 2026 | ||
| Hastelloy C-22HS | Members | 20 Nov 2026 | ||
| Hastelloy G-35 | Members | 20 Nov 2026 | ||
| Hastelloy G-50 / Inconel 050 | Members | 20 Nov 2026 | ||
| Hastelloy G3 | Members | 20 Nov 2026 | ||
| Hastelloy G30 | Members | 20 Nov 2026 | ||
| Hastelloy Hybrid-BC1 | Members | 20 Nov 2026 | ||
| Hastelloy N | Members | 20 Nov 2026 | ||
| Hastelloy S | Members | 20 Nov 2026 | ||
| Hastelloy W | Members | 20 Nov 2026 | ||
| Hastelloy X | Members | 20 Nov 2026 | ||
| Haynes 556 | Members | 20 Nov 2026 | ||
| Haynes HR-120 | Members | 20 Nov 2026 | ||
| Haynes HR-160 | Members | 20 Nov 2026 | ||
| Haynes HR-224 | Members | 20 Nov 2026 | ||
| Haynes HR-235 | Members | 20 Nov 2026 | ||
| Incoloy 25-6MO | Members | 20 Nov 2026 | ||
| Incoloy 800 | Members | 20 Nov 2026 | ||
| Incoloy 800H/HT | Members | 20 Nov 2026 | ||
| Incoloy 803 | Members | 20 Nov 2026 | ||
| Incoloy 825 | Members | 20 Nov 2026 | ||
| Incoloy 864 | Members | 20 Nov 2026 | ||
| Incoloy DS | Members | 20 Nov 2026 | ||
| Inconel 600 | Members | 20 Nov 2026 | ||
| Inconel 601 | Members | 20 Nov 2026 | ||
| Inconel 602CA | Members | 20 Nov 2026 | ||
| Inconel 671 | Members | 20 Nov 2026 | ||
| Inconel 686 | Members | 20 Nov 2026 | ||
| Inconel 690 | Members | 20 Nov 2026 | ||
| Inconel 693 | Members | 20 Nov 2026 | ||
| MO-RE 2 | Members | 20 Nov 2026 | ||
| Monel 400 | Members | 20 Nov 2026 | ||
| Monel 401 | Members | 20 Nov 2026 | ||
| Monel 404 | Members | 20 Nov 2026 | ||
| Monel K-500 | Members | 20 Nov 2026 | ||
| Monel M35-1 (cast) | Members | 20 Nov 2026 | ||
| Na22H | Members | 20 Nov 2026 | ||
| Ni-5Al Thermal Spray | Members | 20 Nov 2026 | ||
| Ni-Be 360 Alloy | Members | 20 Nov 2026 | ||
| Ni-Cr-Mo Dental Ceramic Alloy (Be-free) | Members | 20 Nov 2026 | ||
| Nickel 200/201 | Members | 20 Nov 2026 | ||
| Nickel 211 | Members | 20 Nov 2026 | ||
| Nickel 270 | Members | 20 Nov 2026 | ||
| NiCoCrAlY Bond Coat (Ni-23Co-17Cr-12.5Al-0.5Y) | Members | 20 Nov 2026 | ||
| NiCrAlY Bond Coat (Ni-22Cr-10Al-1Y) | Members | 20 Nov 2026 | ||
| Permanickel 300 | Members | 20 Nov 2026 | ||
| RA 333 | Members | 20 Nov 2026 | ||
| Super Na 22H | Members | 20 Nov 2026 | ||
| Supertherm | Members | 20 Nov 2026 | ||
| Tribaloy T-700 | Members | 20 Nov 2026 |
Nickel Superalloy
110 items| Name | Price USD/kg | Change | 30 days | Published |
|---|---|---|---|---|
| AM1 | Members | 20 Nov 2026 | ||
| AM3 | Members | 20 Nov 2026 | ||
| Astroloy | Members | 20 Nov 2026 | ||
| B-1900 | Members | 20 Nov 2026 | ||
| B-1900 + Hf (PWA 1455) | Members | 20 Nov 2026 | ||
| CM 186 LC | Members | 20 Nov 2026 | ||
| CMSX-10 | Members | 20 Nov 2026 | ||
| CMSX-2 | Members | 20 Nov 2026 | ||
| CMSX-3 | Members | 20 Nov 2026 | ||
| CMSX-4 | Members | 20 Nov 2026 | ||
| CMSX-4 Plus | Members | 20 Nov 2026 | ||
| CMSX-486 | Members | 20 Nov 2026 | ||
| CMSX-6 | Members | 20 Nov 2026 | ||
| CMSX-7 | Members | 20 Nov 2026 | ||
| CMSX-8 | Members | 20 Nov 2026 | ||
| DD6 | Members | 20 Nov 2026 | ||
| EI698 (KhN73MBTYu) | Members | 20 Nov 2026 | ||
| GH3039 (Ni-20Cr-2Mo-1Nb) | Members | 20 Nov 2026 | ||
| GH3044 (Ni-25Cr-15W) | Members | 20 Nov 2026 | ||
| GTD 111 | Members | 20 Nov 2026 | ||
| GTD 222 | Members | 20 Nov 2026 | ||
| GTD-444 | Members | 20 Nov 2026 | ||
| Haynes 214 | Members | 20 Nov 2026 | ||
| Haynes 230 | Members | 20 Nov 2026 | ||
| Haynes 233 | Members | 20 Nov 2026 | ||
| Haynes 242 | Members | 20 Nov 2026 | ||
| Haynes 244 | Members | 20 Nov 2026 | ||
| Haynes 282 | Members | 20 Nov 2026 | ||
| IN-100 | Members | 20 Nov 2026 | ||
| Incoloy 901 | Members | 20 Nov 2026 | ||
| Incoloy 903 | Members | 20 Nov 2026 | ||
| Incoloy 907/909 | Members | 20 Nov 2026 | ||
| Incoloy 925 | Members | 20 Nov 2026 | ||
| Incoloy 945 | Members | 20 Nov 2026 | ||
| Inconel 617 | Members | 20 Nov 2026 | ||
| Inconel 625 (AM) | Members | 20 Nov 2026 | ||
| Inconel 625 (VM) | Members | 20 Nov 2026 | ||
| Inconel 702 | Members | 20 Nov 2026 | ||
| Inconel 706 | Members | 20 Nov 2026 | ||
| Inconel 713LC | Members | 20 Nov 2026 | ||
| Inconel 718 (AM) | Members | 20 Nov 2026 | ||
| Inconel 718 (VM) | Members | 20 Nov 2026 | ||
| Inconel 718+ | Members | 20 Nov 2026 | ||
| Inconel 722 | Members | 20 Nov 2026 | ||
| Inconel 725 | Members | 20 Nov 2026 | ||
| Inconel 738 LC | Members | 20 Nov 2026 | ||
| Inconel 740H | Members | 20 Nov 2026 | ||
| Inconel 751 | Members | 20 Nov 2026 | ||
| Inconel 783 | Members | 20 Nov 2026 | ||
| Inconel 792 | Members | 20 Nov 2026 | ||
| Inconel 939 | Members | 20 Nov 2026 | ||
| Inconel MA6000 | Members | 20 Nov 2026 | ||
| Inconel MA754 | Members | 20 Nov 2026 | ||
| Inconel MA758 | Members | 20 Nov 2026 | ||
| Inconel X-750 | Members | 20 Nov 2026 | ||
| Mar-M 002 | Members | 20 Nov 2026 | ||
| Mar-M 200 | Members | 20 Nov 2026 | ||
| Mar-M 200 + Hf (PWA 1422) | Members | 20 Nov 2026 | ||
| Mar-M 246 | Members | 20 Nov 2026 | ||
| Mar-M 246 + Hf | Members | 20 Nov 2026 | ||
| Mar-M 247 | Members | 20 Nov 2026 | ||
| Mar-M 421 | Members | 20 Nov 2026 | ||
| MC2 | Members | 20 Nov 2026 | ||
| N18 | Members | 20 Nov 2026 | ||
| Nimonic 100 | Members | 20 Nov 2026 | ||
| Nimonic 101 | Members | 20 Nov 2026 | ||
| Nimonic 105 | Members | 20 Nov 2026 | ||
| Nimonic 115 | Members | 20 Nov 2026 | ||
| Nimonic 75 | Members | 20 Nov 2026 | ||
| Nimonic 80A | Members | 20 Nov 2026 | ||
| Nimonic 81 | Members | 20 Nov 2026 | ||
| Nimonic 86 | Members | 20 Nov 2026 | ||
| Nimonic 90 | Members | 20 Nov 2026 | ||
| Nimonic 91 | Members | 20 Nov 2026 | ||
| Nimonic C 263 | Members | 20 Nov 2026 | ||
| Nimonic PE16 | Members | 20 Nov 2026 | ||
| Nimonic PK33 | Members | 20 Nov 2026 | ||
| PWA 1426 | Members | 20 Nov 2026 | ||
| PWA 1480 | Members | 20 Nov 2026 | ||
| PWA 1483 | Members | 20 Nov 2026 | ||
| PWA 1484 | Members | 20 Nov 2026 | ||
| PWA 1487 | Members | 20 Nov 2026 | ||
| Pyromet 31V | Members | 20 Nov 2026 | ||
| Pyromet 860 | Members | 20 Nov 2026 | ||
| Rene 104 | Members | 20 Nov 2026 | ||
| Rene 108 | Members | 20 Nov 2026 | ||
| Rene 125 | Members | 20 Nov 2026 | ||
| Rene 142 | Members | 20 Nov 2026 | ||
| Rene 220 | Members | 20 Nov 2026 | ||
| Rene 41 | Members | 20 Nov 2026 | ||
| Rene 65 | Members | 20 Nov 2026 | ||
| Rene 77 | Members | 20 Nov 2026 | ||
| Rene 80 | Members | 20 Nov 2026 | ||
| Rene 88DT | Members | 20 Nov 2026 | ||
| Rene 95 | Members | 20 Nov 2026 | ||
| Rene N4 | Members | 20 Nov 2026 | ||
| Rene N5 | Members | 20 Nov 2026 | ||
| Rene N500 | Members | 20 Nov 2026 | ||
| Rene N515 | Members | 20 Nov 2026 | ||
| Rene N6 | Members | 20 Nov 2026 | ||
| RR1000 | Members | 20 Nov 2026 | ||
| SRR99 | Members | 20 Nov 2026 | ||
| Udimet 500 | Members | 20 Nov 2026 | ||
| Udimet 520 | Members | 20 Nov 2026 | ||
| Udimet 700 | Members | 20 Nov 2026 | ||
| Udimet 710 | Members | 20 Nov 2026 | ||
| Udimet 720 | Members | 20 Nov 2026 | ||
| Udimet 720Li | Members | 20 Nov 2026 | ||
| Waspaloy | Members | 20 Nov 2026 | ||
| ZhS6U | Members | 20 Nov 2026 |
Precious Alloy
86 items| Name | Price USD/kg | Change | 30 days | Published |
|---|---|---|---|---|
| 800 Silver | Members | 20 Nov 2026 | ||
| 835 Silver | Members | 20 Nov 2026 | ||
| Ag-C 95/5 Contact (Ag-graphite) | Members | 20 Nov 2026 | ||
| Ag-CdO 85/15 Contact | Members | 20 Nov 2026 | ||
| Ag-CdO 90/10 Contact | Members | 20 Nov 2026 | ||
| Ag-Mg-Ni Contact Alloy | Members | 20 Nov 2026 | ||
| Ag-Ni 60/40 Contact | Members | 20 Nov 2026 | ||
| Ag-Ni 90/10 Contact | Members | 20 Nov 2026 | ||
| Ag-Pd 60/40 | Members | 20 Nov 2026 | ||
| Ag-Pd 70/30 | Members | 20 Nov 2026 | ||
| Ag-Pd-Cu-Au Dental Casting Alloy | Members | 20 Nov 2026 | ||
| Ag-SnO2 88/12 Contact | Members | 20 Nov 2026 | ||
| Ag-W 50/50 Contact | Members | 20 Nov 2026 | ||
| Ag-W 65/35 Contact | Members | 20 Nov 2026 | ||
| Ag-WC 60/40 Contact | Members | 20 Nov 2026 | ||
| Ag-ZnO 92/8 Contact | Members | 20 Nov 2026 | ||
| Argentium 935 | Members | 20 Nov 2026 | ||
| Argentium 960 | Members | 20 Nov 2026 | ||
| BAg-1 (45Ag-15Cu-16Zn-24Cd) | Members | 20 Nov 2026 | ||
| BAg-10 (70Ag-20Cu-10Zn) | Members | 20 Nov 2026 | ||
| BAg-13 (54Ag-40Cu-5Zn-1Ni) | Members | 20 Nov 2026 | ||
| BAg-13a (56Ag-42Cu-2Ni) | Members | 20 Nov 2026 | ||
| BAg-18 (60Ag-30Cu-10Sn) | Members | 20 Nov 2026 | ||
| BAg-1a (50Ag-15.5Cu-16.5Zn-18Cd) | Members | 20 Nov 2026 | ||
| BAg-2 (35Ag-26Cu-21Zn-18Cd) | Members | 20 Nov 2026 | ||
| BAg-20 (30Ag-38Cu-32Zn) | Members | 20 Nov 2026 | ||
| BAg-21 (63Ag-28.5Cu-6Sn-2.5Ni) | Members | 20 Nov 2026 | ||
| BAg-22 (49Ag-16Cu-23Zn-7.5Mn-4.5Ni) | Members | 20 Nov 2026 | ||
| BAg-23 (85Ag-15Mn) | Members | 20 Nov 2026 | ||
| BAg-24 (50Ag-20Cu-28Zn-2Ni) | Members | 20 Nov 2026 | ||
| BAg-26 (25Ag-38Cu-33Zn-2Mn-2Ni) | Members | 20 Nov 2026 | ||
| BAg-28 (40Ag-30Cu-28Zn-2Sn) | Members | 20 Nov 2026 | ||
| BAg-3 (50Ag-15.5Cu-15.5Zn-16Cd-3Ni) | Members | 20 Nov 2026 | ||
| BAg-34 (38Ag-32Cu-28Zn-2Sn) | Members | 20 Nov 2026 | ||
| BAg-35 (35Ag-32Cu-33Zn) | Members | 20 Nov 2026 | ||
| BAg-36 (45Ag-27Cu-25Zn-3Sn) | Members | 20 Nov 2026 | ||
| BAg-4 (40Ag-30Cu-28Zn-2Ni) | Members | 20 Nov 2026 | ||
| BAg-5 (45Ag-30Cu-25Zn) | Members | 20 Nov 2026 | ||
| BAg-6 (50Ag-34Cu-16Zn) | Members | 20 Nov 2026 | ||
| BAg-7 (56Ag-22Cu-17Zn-5Sn) | Members | 20 Nov 2026 | ||
| BAg-8 (72Ag-28Cu) | Members | 20 Nov 2026 | ||
| BAg-9 (65Ag-20Cu-15Zn) | Members | 20 Nov 2026 | ||
| Britannia Silver | Members | 20 Nov 2026 | ||
| BVAg-29 (61.5Ag-24Cu-14.5In) | Members | 20 Nov 2026 | ||
| BVAg-30 (68Ag-27Cu-5Pd) | Members | 20 Nov 2026 | ||
| BVAg-31 (58Ag-32Cu-10Pd) | Members | 20 Nov 2026 | ||
| BVAg-32 (54Ag-21Cu-25Pd) | Members | 20 Nov 2026 | ||
| BVAg-6b (50Ag-50Cu) | Members | 20 Nov 2026 | ||
| BVPd-1 (65Pd-35Co) | Members | 20 Nov 2026 | ||
| Coin Silver (900) | Members | 20 Nov 2026 | ||
| Cusil-ABA (63Ag-35.25Cu-1.75Ti) | Members | 20 Nov 2026 | ||
| Dental Amalgam Alloy (Ag-Sn-Cu) | Members | 20 Nov 2026 | ||
| Dental Amalgam Alloy (High-Cu) | Members | 20 Nov 2026 | ||
| Incusil-ABA (59Ag-27.25Cu-12.5In-1.25Ti) | Members | 20 Nov 2026 | ||
| Ir-Pt 70/30 | Members | 20 Nov 2026 | ||
| Ir-Rh 60/40 | Members | 20 Nov 2026 | ||
| Pd-Ag 60/40 | Members | 20 Nov 2026 | ||
| Pd-Ag 70/30 | Members | 20 Nov 2026 | ||
| Pd-Ag 77/23 | Members | 20 Nov 2026 | ||
| Pd-Ag Ceramic Alloy (Dental) | Members | 20 Nov 2026 | ||
| Pd-Co 95/5 | Members | 20 Nov 2026 | ||
| Pd-Cu 60/40 | Members | 20 Nov 2026 | ||
| Pd-Cu-Ga Ceramic Alloy (Dental) | Members | 20 Nov 2026 | ||
| Pd-Ni 80/20 | Members | 20 Nov 2026 | ||
| Pd-Ru 95/5 | Members | 20 Nov 2026 | ||
| Pt-Au 95/5 | Members | 20 Nov 2026 | ||
| Pt-Co 95/5 | Members | 20 Nov 2026 | ||
| Pt-Cu 95/5 | Members | 20 Nov 2026 | ||
| Pt-Ir 70/30 | Members | 20 Nov 2026 | ||
| Pt-Ir 80/20 | Members | 20 Nov 2026 | ||
| Pt-Ir 85/15 | Members | 20 Nov 2026 | ||
| Pt-Ir 90/10 | Members | 20 Nov 2026 | ||
| Pt-Ir 95/5 | Members | 20 Nov 2026 | ||
| Pt-Ni 95/5 | Members | 20 Nov 2026 | ||
| Pt-Pd 95/5 | Members | 20 Nov 2026 | ||
| Pt-Rh 70/30 | Members | 20 Nov 2026 | ||
| Pt-Rh 80/20 | Members | 20 Nov 2026 | ||
| Pt-Rh 87/13 | Members | 20 Nov 2026 | ||
| Pt-Rh 90/10 | Members | 20 Nov 2026 | ||
| Pt-Rh 94/6 | Members | 20 Nov 2026 | ||
| Pt-Rh 95/5 | Members | 20 Nov 2026 | ||
| Pt-Ru 90/10 | Members | 20 Nov 2026 | ||
| Pt-Ru 95/5 | Members | 20 Nov 2026 | ||
| Pt-W 92/8 | Members | 20 Nov 2026 | ||
| Sterling Silver | Members | 20 Nov 2026 | ||
| Ticusil (68.8Ag-26.7Cu-4.5Ti) | Members | 20 Nov 2026 |
Rare Earths
15 items| Name | Price USD/kg | Change | 30 days | Published |
|---|---|---|---|---|
| Ce(Cerium) | Members | 20 Nov 2026 | ||
| Dy (Dysprosium) | Members | 20 Nov 2026 | ||
| Er (Erbium) | Members | 20 Nov 2026 | ||
| Eu (Europium) | Members | 20 Nov 2026 | ||
| Gd (Gadolinium) | Members | 20 Nov 2026 | ||
| Ho (Holmium) | Members | 20 Nov 2026 | ||
| La (Lanthanum) | Members | 20 Nov 2026 | ||
| Lu (Lutetium) | Members | 20 Nov 2026 | ||
| Mm (Mischmetal) | Members | 20 Nov 2026 | ||
| Nd (Neodymium) | Members | 20 Nov 2026 | ||
| Pr (Praseodymium) | Members | 20 Nov 2026 | ||
| Sm (Samarium) | Members | 20 Nov 2026 | ||
| Tb (Terbium) | Members | 20 Nov 2026 | ||
| Y (Yttrium) | Members | 20 Nov 2026 | ||
| Yb (Ytterbium) | Members | 20 Nov 2026 |
Refractory Alloy
53 items| Name | Price USD/kg | Change | 30 days | Published |
|---|---|---|---|---|
| 90W-6Ni-4Cu | Members | 20 Nov 2026 | ||
| 90W-7Ni-3Fe | Members | 20 Nov 2026 | ||
| 92.5W-5.25Ni-2.25Fe | Members | 20 Nov 2026 | ||
| 93W-5Ni-2Fe | Members | 20 Nov 2026 | ||
| 95W-3.5Ni-1.5Cu | Members | 20 Nov 2026 | ||
| 95W-3.5Ni-1.5Fe | Members | 20 Nov 2026 | ||
| 97W-2.1Ni-0.9Fe | Members | 20 Nov 2026 | ||
| Anviloy 1150 | Members | 20 Nov 2026 | ||
| C-103 | Members | 20 Nov 2026 | ||
| C-129Y | Members | 20 Nov 2026 | ||
| Cb-752 | Members | 20 Nov 2026 | ||
| E635 | Members | 20 Nov 2026 | ||
| FS-85 | Members | 20 Nov 2026 | ||
| MHC | Members | 20 Nov 2026 | ||
| Mo-30W | Members | 20 Nov 2026 | ||
| Mo-41Re | Members | 20 Nov 2026 | ||
| Mo-47.5Re | Members | 20 Nov 2026 | ||
| Mo-50W | Members | 20 Nov 2026 | ||
| Mo-Cu 50/50 | Members | 20 Nov 2026 | ||
| Mo-Cu 70/30 | Members | 20 Nov 2026 | ||
| Mo-Cu 85/15 | Members | 20 Nov 2026 | ||
| Mo-La (ML) | Members | 20 Nov 2026 | ||
| Nb-1Zr | Members | 20 Nov 2026 | ||
| Nb-47Ti | Members | 20 Nov 2026 | ||
| Nb-521 | Members | 20 Nov 2026 | ||
| Nb3Sn | Members | 20 Nov 2026 | ||
| T-111 | Members | 20 Nov 2026 | ||
| Ta-10W | Members | 20 Nov 2026 | ||
| Ta-2.5W | Members | 20 Nov 2026 | ||
| Ta-40Nb | Members | 20 Nov 2026 | ||
| Ta-7.5W | Members | 20 Nov 2026 | ||
| TZC | Members | 20 Nov 2026 | ||
| TZM | Members | 20 Nov 2026 | ||
| W-25Re | Members | 20 Nov 2026 | ||
| W-26Re | Members | 20 Nov 2026 | ||
| W-3Re | Members | 20 Nov 2026 | ||
| W-5Re | Members | 20 Nov 2026 | ||
| W-Cu 50/50 | Members | 20 Nov 2026 | ||
| W-Cu 60/40 | Members | 20 Nov 2026 | ||
| W-Cu 70/30 | Members | 20 Nov 2026 | ||
| W-Cu 75/25 | Members | 20 Nov 2026 | ||
| W-Cu 80/20 | Members | 20 Nov 2026 | ||
| W-Cu 90/10 | Members | 20 Nov 2026 | ||
| WC-3009 | Members | 20 Nov 2026 | ||
| WC20 | Members | 20 Nov 2026 | ||
| WL10 | Members | 20 Nov 2026 | ||
| WL15 | Members | 20 Nov 2026 | ||
| Zircaloy-2 | Members | 20 Nov 2026 | ||
| Zircaloy-4 | Members | 20 Nov 2026 | ||
| ZIRLO-type Zr-1Nb-1Sn | Members | 20 Nov 2026 | ||
| Zr 702 | Members | 20 Nov 2026 | ||
| Zr-1Nb | Members | 20 Nov 2026 | ||
| Zr-2.5Nb | Members | 20 Nov 2026 |
Special Metal
25 items| Name | Price USD/kg | Change | 30 days | Published |
|---|---|---|---|---|
| Bi Bismuth | Members | 20 Nov 2026 | ||
| C(Graphite) | Members | 20 Nov 2026 | ||
| Cd Cadmium | Members | 20 Nov 2026 | ||
| Co Cobalt | Members | 20 Nov 2026 | ||
| Cr Chromium | Members | 20 Nov 2026 | ||
| Ga Gallium | Members | 20 Nov 2026 | ||
| Ge Germanium | Members | 20 Nov 2026 | ||
| Hf Hafnium | Members | 20 Nov 2026 | ||
| In Indium | Members | 20 Nov 2026 | ||
| Li Lithium | Members | 20 Nov 2026 | ||
| Mg Magnesium | Members | 20 Nov 2026 | ||
| Mn Manganese | Members | 20 Nov 2026 | ||
| Mo Molybdenum | Members | 20 Nov 2026 | ||
| Mo (Air) | Members | 20 Nov 2026 | ||
| Mo(Ox) | Members | 20 Nov 2026 | ||
| Nb(Vac) | Members | 20 Nov 2026 | ||
| Re Rhenium | Members | 20 Nov 2026 | ||
| Se Selenium | Members | 20 Nov 2026 | ||
| Si Silicon | Members | 20 Nov 2026 | ||
| Ta Tantalum | Members | 20 Nov 2026 | ||
| Te Tellurium | Members | 20 Nov 2026 | ||
| Ti Titanium | Members | 20 Nov 2026 | ||
| V Vanadium | Members | 20 Nov 2026 | ||
| W Tungsten | Members | 20 Nov 2026 | ||
| Zr (Hf) | Members | 20 Nov 2026 |
Stainless
137 items| Name | Price USD/kg | Change | 30 days | Published |
|---|---|---|---|---|
| 1.2316 (X38CrMo16) | Members | 20 Nov 2026 | ||
| 1.4112 (X90CrMoV18) | Members | 20 Nov 2026 | ||
| 1.4116 (X50CrMoV15) | Members | 20 Nov 2026 | ||
| 1.4435 (316L 2.5Mo / 316LVM) | Members | 20 Nov 2026 | ||
| 1.4742 (X10CrAlSi18) | Members | 20 Nov 2026 | ||
| 1.4762 (X10CrAlSi25) | Members | 20 Nov 2026 | ||
| 1.4828 (X15CrNiSi20-12) | Members | 20 Nov 2026 | ||
| 13-8 MO | Members | 20 Nov 2026 | ||
| 13Cr-4Ni (F6NM / CA6NM) | Members | 20 Nov 2026 | ||
| 15-5 PH | Members | 20 Nov 2026 | ||
| 154CM | Members | 20 Nov 2026 | ||
| 16-5-1 (1.4418) | Members | 20 Nov 2026 | ||
| 17-4 PH | Members | 20 Nov 2026 | ||
| 17-7 PH | Members | 20 Nov 2026 | ||
| 2003 | Members | 20 Nov 2026 | ||
| 201 | Members | 20 Nov 2026 | ||
| 202 | Members | 20 Nov 2026 | ||
| 204Cu | Members | 20 Nov 2026 | ||
| 205 | Members | 20 Nov 2026 | ||
| 21-2N (EV12 valve steel) | Members | 20 Nov 2026 | ||
| 21-4N (EV8 valve steel) | Members | 20 Nov 2026 | ||
| 2101 (LDX 2101) | Members | 20 Nov 2026 | ||
| 2102 | Members | 20 Nov 2026 | ||
| 2202 | Members | 20 Nov 2026 | ||
| 2205 Duplex | Members | 20 Nov 2026 | ||
| 23-8N (EV16 valve steel) | Members | 20 Nov 2026 | ||
| 2304 | Members | 20 Nov 2026 | ||
| 2404 (LDX 2404) | Members | 20 Nov 2026 | ||
| 2507 Duplex | Members | 20 Nov 2026 | ||
| 253 MA | Members | 20 Nov 2026 | ||
| 254SMO | Members | 20 Nov 2026 | ||
| 255 (Ferralium) | Members | 20 Nov 2026 | ||
| 2707 HD | Members | 20 Nov 2026 | ||
| 29-4-2 | Members | 20 Nov 2026 | ||
| 29-4C | Members | 20 Nov 2026 | ||
| 2906 (Hyper Duplex) | Members | 20 Nov 2026 | ||
| 301 | Members | 20 Nov 2026 | ||
| 302HQ (XM-7) | Members | 20 Nov 2026 | ||
| 304 | Members | 20 Nov 2026 | ||
| 304 L | Members | 20 Nov 2026 | ||
| 304H | Members | 20 Nov 2026 | ||
| 305 | Members | 20 Nov 2026 | ||
| 308 | Members | 20 Nov 2026 | ||
| 309 | Members | 20 Nov 2026 | ||
| 309 S | Members | 20 Nov 2026 | ||
| 310 | Members | 20 Nov 2026 | ||
| 310 S | Members | 20 Nov 2026 | ||
| 310MoLN | Members | 20 Nov 2026 | ||
| 316 | Members | 20 Nov 2026 | ||
| 316 L | Members | 20 Nov 2026 | ||
| 316Ti | Members | 20 Nov 2026 | ||
| 317 | Members | 20 Nov 2026 | ||
| 317L | Members | 20 Nov 2026 | ||
| 317LMN | Members | 20 Nov 2026 | ||
| 321 | Members | 20 Nov 2026 | ||
| 329 | Members | 20 Nov 2026 | ||
| 330 | Members | 20 Nov 2026 | ||
| 347 | Members | 20 Nov 2026 | ||
| 353 MA | Members | 20 Nov 2026 | ||
| 35Ni25CrNb | Members | 20 Nov 2026 | ||
| 384 | Members | 20 Nov 2026 | ||
| 3CR12 (1.4003) | Members | 20 Nov 2026 | ||
| 403 | Members | 20 Nov 2026 | ||
| 405 | Members | 20 Nov 2026 | ||
| 409 | Members | 20 Nov 2026 | ||
| 410 | Members | 20 Nov 2026 | ||
| 410L (SUS410L) | Members | 20 Nov 2026 | ||
| 414 | Members | 20 Nov 2026 | ||
| 418 (Greek Ascoloy) | Members | 20 Nov 2026 | ||
| 420 | Members | 20 Nov 2026 | ||
| 422 | Members | 20 Nov 2026 | ||
| 429 | Members | 20 Nov 2026 | ||
| 430 | Members | 20 Nov 2026 | ||
| 431 | Members | 20 Nov 2026 | ||
| 434 | Members | 20 Nov 2026 | ||
| 436 | Members | 20 Nov 2026 | ||
| 439 | Members | 20 Nov 2026 | ||
| 440A | Members | 20 Nov 2026 | ||
| 440C | Members | 20 Nov 2026 | ||
| 441 | Members | 20 Nov 2026 | ||
| 442 | Members | 20 Nov 2026 | ||
| 444 | Members | 20 Nov 2026 | ||
| 446 | Members | 20 Nov 2026 | ||
| 904 L | Members | 20 Nov 2026 | ||
| A 286 | Members | 20 Nov 2026 | ||
| AL 6XN | Members | 20 Nov 2026 | ||
| AM-350 | Members | 20 Nov 2026 | ||
| AM-355 | Members | 20 Nov 2026 | ||
| CD4MCu | Members | 20 Nov 2026 | ||
| CF3M | Members | 20 Nov 2026 | ||
| CF8 | Members | 20 Nov 2026 | ||
| CF8M | Members | 20 Nov 2026 | ||
| CG8M | Members | 20 Nov 2026 | ||
| CN7M | Members | 20 Nov 2026 | ||
| CPM S30V | Members | 20 Nov 2026 | ||
| CPM S35VN | Members | 20 Nov 2026 | ||
| CPM S90V | Members | 20 Nov 2026 | ||
| Custom 450 | Members | 20 Nov 2026 | ||
| Custom 455 | Members | 20 Nov 2026 | ||
| Custom 465 | Members | 20 Nov 2026 | ||
| DP-3W | Members | 20 Nov 2026 | ||
| E-Brite 26-1 | Members | 20 Nov 2026 | ||
| HC | Members | 20 Nov 2026 | ||
| HD | Members | 20 Nov 2026 | ||
| HE | Members | 20 Nov 2026 | ||
| HH | Members | 20 Nov 2026 | ||
| HI | Members | 20 Nov 2026 | ||
| HK40 | Members | 20 Nov 2026 | ||
| HL | Members | 20 Nov 2026 | ||
| HN | Members | 20 Nov 2026 | ||
| HP | Members | 20 Nov 2026 | ||
| HR3C (S31042) | Members | 20 Nov 2026 | ||
| HT | Members | 20 Nov 2026 | ||
| HU | Members | 20 Nov 2026 | ||
| HW | Members | 20 Nov 2026 | ||
| HX | Members | 20 Nov 2026 | ||
| Jethete M152 | Members | 20 Nov 2026 | ||
| M390 (Bohler PM) | Members | 20 Nov 2026 | ||
| MO-RE 1 | Members | 20 Nov 2026 | ||
| N-155 | Members | 20 Nov 2026 | ||
| N690 (Bohler) | Members | 20 Nov 2026 | ||
| Nitronic 30 | Members | 20 Nov 2026 | ||
| Nitronic 32 (18-2Mn) | Members | 20 Nov 2026 | ||
| Nitronic 33 (18-3Mn) | Members | 20 Nov 2026 | ||
| Nitronic 40 (21-6-9) | Members | 20 Nov 2026 | ||
| Nitronic 50 (XM-19) | Members | 20 Nov 2026 | ||
| Nitronic 60 | Members | 20 Nov 2026 | ||
| P122 (HCM12A) | Members | 20 Nov 2026 | ||
| PH 14-8 Mo | Members | 20 Nov 2026 | ||
| PH 15-7 Mo | Members | 20 Nov 2026 | ||
| Pyrowear 675 | Members | 20 Nov 2026 | ||
| Sea-Cure | Members | 20 Nov 2026 | ||
| SUH3 (X40CrSiMo10-2 valve steel) | Members | 20 Nov 2026 | ||
| Super 304H (S30432) | Members | 20 Nov 2026 | ||
| VG-10 | Members | 20 Nov 2026 | ||
| X20CrMoV12-1 | Members | 20 Nov 2026 | ||
| Zeron 100 | Members | 20 Nov 2026 |
Steel
79 items| Name | Price USD/kg | Change | 30 days | Published |
|---|---|---|---|---|
| 1.25Cr-0.5Mo (P11) | Members | 20 Nov 2026 | ||
| 100CrMo7 (1.3537) | Members | 20 Nov 2026 | ||
| 1018 | Members | 20 Nov 2026 | ||
| 1045 | Members | 20 Nov 2026 | ||
| 12Cr1MoV (GB boiler steel) | Members | 20 Nov 2026 | ||
| 12L14 (leaded free-cutting) | Members | 20 Nov 2026 | ||
| 15Cr-Mo White Iron (A532 II-B) | Members | 20 Nov 2026 | ||
| 16Mo3 (1.5415) | Members | 20 Nov 2026 | ||
| 18CrNiMo7-6 | Members | 20 Nov 2026 | ||
| 2.25Cr-1.6W (P23) | Members | 20 Nov 2026 | ||
| 2.25Cr-1Mo (P22) | Members | 20 Nov 2026 | ||
| 2.25Ni Steel (A203 Gr.A/B) | Members | 20 Nov 2026 | ||
| 2.4Cr-1Mo-V (P24) | Members | 20 Nov 2026 | ||
| 20MnCr5 (1.7147) | Members | 20 Nov 2026 | ||
| 25Cr White Iron (A532 III-A) | Members | 20 Nov 2026 | ||
| 3.5Ni Steel | Members | 20 Nov 2026 | ||
| 300M | Members | 20 Nov 2026 | ||
| 30CrNiMo8 (1.6580) | Members | 20 Nov 2026 | ||
| 34CrNiMo6 (1.6582) | Members | 20 Nov 2026 | ||
| 4130 | Members | 20 Nov 2026 | ||
| 4140 | Members | 20 Nov 2026 | ||
| 4320 | Members | 20 Nov 2026 | ||
| 4330V (Mod) | Members | 20 Nov 2026 | ||
| 4340 | Members | 20 Nov 2026 | ||
| 4620 | Members | 20 Nov 2026 | ||
| 4820 | Members | 20 Nov 2026 | ||
| 5160 | Members | 20 Nov 2026 | ||
| 52100 | Members | 20 Nov 2026 | ||
| 5Cr-0.5Mo (P5) | Members | 20 Nov 2026 | ||
| 5Ni Steel (A645) | Members | 20 Nov 2026 | ||
| 8620 | Members | 20 Nov 2026 | ||
| 9310 | Members | 20 Nov 2026 | ||
| 9Cr-1Mo (P9) | Members | 20 Nov 2026 | ||
| 9Ni Steel | Members | 20 Nov 2026 | ||
| A242 (Cor-Ten A type) | Members | 20 Nov 2026 | ||
| A514 Gr.B (T-1 type) | Members | 20 Nov 2026 | ||
| A514 Gr.Q | Members | 20 Nov 2026 | ||
| A588 Weathering | Members | 20 Nov 2026 | ||
| Aermet 100 | Members | 20 Nov 2026 | ||
| Aermet 310 | Members | 20 Nov 2026 | ||
| AF1410 | Members | 20 Nov 2026 | ||
| D6AC | Members | 20 Nov 2026 | ||
| Ductile Cast Iron (A536 65-45-12) | Members | 20 Nov 2026 | ||
| Ferrium C64 | Members | 20 Nov 2026 | ||
| Ferrium M54 | Members | 20 Nov 2026 | ||
| Ferrium S53 | Members | 20 Nov 2026 | ||
| Grey Cast Iron (A48 Class 30) | Members | 20 Nov 2026 | ||
| Hadfield Mn Steel | Members | 20 Nov 2026 | ||
| High-Mn Cryogenic Steel (A1106) | Members | 20 Nov 2026 | ||
| High-Si Iron (A518 Gr.1 / Duriron type) | Members | 20 Nov 2026 | ||
| HP 9-4-30 | Members | 20 Nov 2026 | ||
| HSLA-100 | Members | 20 Nov 2026 | ||
| HSLA-80 (A710 Gr.A) | Members | 20 Nov 2026 | ||
| HY-100 | Members | 20 Nov 2026 | ||
| HY-130 | Members | 20 Nov 2026 | ||
| HY-80 | Members | 20 Nov 2026 | ||
| M50 Bearing Steel | Members | 20 Nov 2026 | ||
| M50NiL | Members | 20 Nov 2026 | ||
| Maraging 200 | Members | 20 Nov 2026 | ||
| Maraging 250 | Members | 20 Nov 2026 | ||
| Maraging 300 | Members | 20 Nov 2026 | ||
| Maraging 350 | Members | 20 Nov 2026 | ||
| Maraging T-250 (Co-free) | Members | 20 Nov 2026 | ||
| Ni-Hard 1 (A532 I-A) | Members | 20 Nov 2026 | ||
| Ni-Hard 4 (A532 I-D) | Members | 20 Nov 2026 | ||
| Ni-Resist 1 | Members | 20 Nov 2026 | ||
| Ni-Resist 2 | Members | 20 Nov 2026 | ||
| Ni-Resist 3 | Members | 20 Nov 2026 | ||
| Ni-Resist 4 | Members | 20 Nov 2026 | ||
| Ni-Resist 5 | Members | 20 Nov 2026 | ||
| Nitralloy 135M | Members | 20 Nov 2026 | ||
| P1 (C-0.5Mo) | Members | 20 Nov 2026 | ||
| P12 (1Cr-0.5Mo) | Members | 20 Nov 2026 | ||
| P36 (15NiCuMoNb5-6-4 / WB36) | Members | 20 Nov 2026 | ||
| P91 (9Cr-1Mo-V) | Members | 20 Nov 2026 | ||
| P92 (9Cr-0.5Mo-2W) | Members | 20 Nov 2026 | ||
| Pyrowear 53 | Members | 20 Nov 2026 | ||
| SA-508 Gr.3 (Mn-Ni-Mo RPV) | Members | 20 Nov 2026 | ||
| SUH1 (X45CrSi9-3 valve steel) | Members | 20 Nov 2026 |
Ti Alloy
93 items| Name | Price USD/kg | Change | 30 days | Published |
|---|---|---|---|---|
| Beta III | Members | 20 Nov 2026 | ||
| IMI 550 | Members | 20 Nov 2026 | ||
| IMI 551 | Members | 20 Nov 2026 | ||
| IMI 679 | Members | 20 Nov 2026 | ||
| IMI 685 | Members | 20 Nov 2026 | ||
| IMI 829 | Members | 20 Nov 2026 | ||
| OT4 | Members | 20 Nov 2026 | ||
| OT4-1 (Ti-2Al-1.5Mn) | Members | 20 Nov 2026 | ||
| PT-7M (Ti-2.2Al-2.5Zr) | Members | 20 Nov 2026 | ||
| SP-700 | Members | 20 Nov 2026 | ||
| TA15 | Members | 20 Nov 2026 | ||
| TB2 | Members | 20 Nov 2026 | ||
| TC11 | Members | 20 Nov 2026 | ||
| TC21 | Members | 20 Nov 2026 | ||
| Ti -15Zr | Members | 20 Nov 2026 | ||
| Ti 15-3-3-3 | Members | 20 Nov 2026 | ||
| Ti 6-2-2-2-2 | Members | 20 Nov 2026 | ||
| Ti 6-2-4-2 | Members | 20 Nov 2026 | ||
| Ti Cp Gr.1 | Members | 20 Nov 2026 | ||
| Ti Cp Gr.2 | Members | 20 Nov 2026 | ||
| Ti Cp Gr.2H | Members | 20 Nov 2026 | ||
| Ti Cp Gr.3 | Members | 20 Nov 2026 | ||
| Ti Cp Gr.4 | Members | 20 Nov 2026 | ||
| Ti Gr.11 (Pd) | Members | 20 Nov 2026 | ||
| Ti Gr.12 (Ni) | Members | 20 Nov 2026 | ||
| Ti Gr.13 | Members | 20 Nov 2026 | ||
| Ti Gr.14 | Members | 20 Nov 2026 | ||
| Ti Gr.15 | Members | 20 Nov 2026 | ||
| Ti Gr.16 (Pd) | Members | 20 Nov 2026 | ||
| Ti Gr.17 | Members | 20 Nov 2026 | ||
| Ti Gr.18 | Members | 20 Nov 2026 | ||
| Ti Gr.19 (Beta-C) | Members | 20 Nov 2026 | ||
| Ti Gr.20 | Members | 20 Nov 2026 | ||
| Ti Gr.21 | Members | 20 Nov 2026 | ||
| Ti Gr.23 (ELI) | Members | 20 Nov 2026 | ||
| Ti Gr.24 | Members | 20 Nov 2026 | ||
| Ti Gr.25 | Members | 20 Nov 2026 | ||
| Ti Gr.26 | Members | 20 Nov 2026 | ||
| Ti Gr.27 | Members | 20 Nov 2026 | ||
| Ti Gr.28 | Members | 20 Nov 2026 | ||
| Ti Gr.29 | Members | 20 Nov 2026 | ||
| Ti Gr.30 | Members | 20 Nov 2026 | ||
| Ti Gr.31 | Members | 20 Nov 2026 | ||
| Ti Gr.32 | Members | 20 Nov 2026 | ||
| Ti Gr.33 | Members | 20 Nov 2026 | ||
| Ti Gr.34 | Members | 20 Nov 2026 | ||
| Ti Gr.35 | Members | 20 Nov 2026 | ||
| Ti Gr.36 | Members | 20 Nov 2026 | ||
| Ti Gr.37 | Members | 20 Nov 2026 | ||
| Ti Gr.38 | Members | 20 Nov 2026 | ||
| Ti Gr.39 | Members | 20 Nov 2026 | ||
| Ti Gr.40 | Members | 20 Nov 2026 | ||
| Ti Gr.5 (6Al4V) | Members | 20 Nov 2026 | ||
| Ti Gr.6 | Members | 20 Nov 2026 | ||
| Ti Gr.7 (Pd) | Members | 20 Nov 2026 | ||
| Ti Gr.9 | Members | 20 Nov 2026 | ||
| Ti-10V-2Fe-3Al | Members | 20 Nov 2026 | ||
| Ti-12Mo-6Zr-2Fe | Members | 20 Nov 2026 | ||
| Ti-13Nb-13Zr | Members | 20 Nov 2026 | ||
| Ti-13V-11Cr-3Al | Members | 20 Nov 2026 | ||
| Ti-15Mo | Members | 20 Nov 2026 | ||
| Ti-15Mo-5Zr-3Al | Members | 20 Nov 2026 | ||
| Ti-185 | Members | 20 Nov 2026 | ||
| Ti-2.5Cu | Members | 20 Nov 2026 | ||
| Ti-35Nb-7Zr-5Ta | Members | 20 Nov 2026 | ||
| Ti-35V-15Cr (Alloy C) | Members | 20 Nov 2026 | ||
| Ti-5.8Al-4Sn-3.5Zr-0.7Nb-0.5Mo-0.35Si-0.06C (834) | Members | 20 Nov 2026 | ||
| Ti-54M | Members | 20 Nov 2026 | ||
| Ti-55511 (VT22) | Members | 20 Nov 2026 | ||
| Ti-5553 | Members | 20 Nov 2026 | ||
| Ti-5621S | Members | 20 Nov 2026 | ||
| Ti-5Al-2.5Fe | Members | 20 Nov 2026 | ||
| Ti-5Al-2.5Sn ELI | Members | 20 Nov 2026 | ||
| Ti-5Al-2Sn-4Zr-4Mo-4Cr (Ti-17) | Members | 20 Nov 2026 | ||
| Ti-6Al-2.7Sn-4Zr-0.4Mo-0.45Si (1100) | Members | 20 Nov 2026 | ||
| Ti-6Al-2Nb-1Ta-0.8Mo | Members | 20 Nov 2026 | ||
| Ti-6Al-2Sn-4Zr-6Mo (6246) | Members | 20 Nov 2026 | ||
| Ti-6Al-6V-2Sn | Members | 20 Nov 2026 | ||
| Ti-6Al-7Nb | Members | 20 Nov 2026 | ||
| Ti-7Al-4Mo | Members | 20 Nov 2026 | ||
| Ti-8-1-1 | Members | 20 Nov 2026 | ||
| Ti-8Mn | Members | 20 Nov 2026 | ||
| TiAl 48-2-2 | Members | 20 Nov 2026 | ||
| TIMETAL 62S | Members | 20 Nov 2026 | ||
| TIMETAL LCB | Members | 20 Nov 2026 | ||
| TNM | Members | 20 Nov 2026 | ||
| VT14 | Members | 20 Nov 2026 | ||
| VT16 | Members | 20 Nov 2026 | ||
| VT18U | Members | 20 Nov 2026 | ||
| VT23 | Members | 20 Nov 2026 | ||
| VT3-1 | Members | 20 Nov 2026 | ||
| VT5 (Ti-5Al) | Members | 20 Nov 2026 | ||
| VT8 | Members | 20 Nov 2026 |
Tool Steel
33 items| Name | Price USD/kg | Change | 30 days | Published |
|---|---|---|---|---|
| 1.2367 (X38CrMoV5-3) | Members | 20 Nov 2026 | ||
| 1.2714 (55NiCrMoV7 / SKT4) | Members | 20 Nov 2026 | ||
| 1.2738 (P20+Ni) | Members | 20 Nov 2026 | ||
| 1.2767 (45NiCrMo16) | Members | 20 Nov 2026 | ||
| 1.2842 (90MnCrV8 / O2) | Members | 20 Nov 2026 | ||
| A2 | Members | 20 Nov 2026 | ||
| A8 | Members | 20 Nov 2026 | ||
| ASP 2030 (PM HSS, M3:2+Co) | Members | 20 Nov 2026 | ||
| ASP 2060 (PM HSS) | Members | 20 Nov 2026 | ||
| CPM 10V (A11) | Members | 20 Nov 2026 | ||
| D2 | Members | 20 Nov 2026 | ||
| D3 | Members | 20 Nov 2026 | ||
| H10 (1.2365) | Members | 20 Nov 2026 | ||
| H11 | Members | 20 Nov 2026 | ||
| H13 | Members | 20 Nov 2026 | ||
| H21 | Members | 20 Nov 2026 | ||
| L6 | Members | 20 Nov 2026 | ||
| M1 | Members | 20 Nov 2026 | ||
| M2 | Members | 20 Nov 2026 | ||
| M3 Class 2 | Members | 20 Nov 2026 | ||
| M35 | Members | 20 Nov 2026 | ||
| M4 | Members | 20 Nov 2026 | ||
| M42 | Members | 20 Nov 2026 | ||
| M7 | Members | 20 Nov 2026 | ||
| NAK80 (P21 type) | Members | 20 Nov 2026 | ||
| O1 | Members | 20 Nov 2026 | ||
| P20 | Members | 20 Nov 2026 | ||
| S1 | Members | 20 Nov 2026 | ||
| S7 | Members | 20 Nov 2026 | ||
| SKS3 | Members | 20 Nov 2026 | ||
| T1 | Members | 20 Nov 2026 | ||
| T15 | Members | 20 Nov 2026 | ||
| W2 | Members | 20 Nov 2026 |
Movers
Up
In the data
What members get
- All 1,185 prices, every business day (1,121 alloys, 64 materials)
- Each alloy's recipe: share × material price, line by line
- Corrections recorded with their reasons
All 1,185 prices, every business day
Every material and alloy, the full history and each alloy priced line by line from its recipe.
Start free trialYour first purchase is refunded in full if you ask within 14 days.
About these prices
- Every price is in US dollars per kilogram (USD/kg).
- SuperMetalPrice publishes one value per item per business day, normally by 20:30 New York time (ET) on the evening before the price date, after an approval step. A change compares an item with its previous published price.
- Each alloy price is calculated from the published prices of its materials and its recipe, the share of each material in it.
- Prices are daily published values, not live quotes or offers to buy or sell.